Solid Carbide 2/4 Flute Square End Mill Flat End Mill for Process Aluminum Alloy/Harden Steel/Stainless Steel/Nickel-Based High Superalloy

Solid Carbide 2/4 Flute Square End Mill Flat End Mill for Process Aluminum Alloy/Harden Steel/Stainless Steel/Nickel-Based High Superalloy

Specifications: 1.Hardness:HRC45/50/55/60/65 2.Flutes:2 flutes or 4 flutes 3.Helix Angle: 35 degree 4.Centered Cutting:
SHARE

Description

Basic Info
Model NO. End mill
Usage Scenarios CNC Machine
Usage Scenarios2 Machining Center
Usage Scenarios3 Lathe Turning Machine
Transport Package Box
Trademark Quander
Origin China
HS Code 8208101900
Production Capacity 1000000PCS/Year
Product Description
Specifications:

1.Hardness:HRC45/50/55/60/65
2.Flutes:2 flutes or 4 flutes
3.Helix Angle: 35 degree
4.Centered Cutting: Yes
5.Type: Square End Mill / Flat end mill / Metal cutting tool
6.Workpiece material: Steel, mould steel, low alloy, hardened steel, staninless steel, alloy steel
7.Coating:TiAlN
8.Tool body material:Tungsten solid carbide
9.Color: Black, yellow

Description of solid carbide end mills ,CNC end mill ,hardness end mill

Flutes No.2/3/4 Flutes
MaterialHSS,Carbide etc.
CoatingAlTiN,NACO BLUE/NACO BLACK/TiN etc.
Helix Angle35°,45°
HardnessHRC45/55/58/65
SizeOveral Length:50-150mm
CustomizedAccept
Smooth FinishHighly Polished
FeatureExcellent chip evacuation
MeasurementMetric

Super raw material

HRC45HRC55HRC60HRC65
YG10XYG10.2 &WF25(Taiwan)K44 & K40 (German)H10F (Sweden)
Grain Size:0.7um
Co:10 %
Flexural strength:3320N/mm2
Grain Size:0.6um
Co:10 %
Flexural strength:4000N/mm2
Grain Size:0.5um
Co:12 %
Flexural strength:4300N/mm2
Grain Size:0.5um
Co:10 %
Flexural strength:4300N/mm2

Super coating

ItemAlTiNTiAINTiSiNNACO
Hardness(HV)32002800360042(GPA)
Thickness(UM)2.5-32.5-333
Oxidation Temp(°)90080010001200
Friction Coeffient0.30.30.450.4
ColorBlackVioletCopperBlue